Electronic Theses and Dissertation
Universitas Syiah Kuala
SKRIPSI
PENGARUH PENAMBAHAN NANOPARTIKEL ZIRKONIA TERHADAP FLEXURAL STRENGTH BASISRN GIGI TIRUAN REPARASI
Pengarang
Teuku Shaumal Hasaan - Personal Name;
Dosen Pembimbing
Syahrial - 198510152015041002 - Dosen Pembimbing I
Liana Rahmayani - 197409192002122006 - Dosen Pembimbing II
Nomor Pokok Mahasiswa
2213101010048
Fakultas & Prodi
Fakultas Kedokteran Gigi / Pendidikan Dokter Gigi (S1) / PDDIKTI : 12201
Subject
Kata Kunci
Penerbit
Banda Aceh : Fakultas Kedokteran Gigi., 2026
Bahasa
No Classification
-
Literature Searching Service
Hard copy atau foto copy dari buku ini dapat diberikan dengan syarat ketentuan berlaku, jika berminat, silahkan hubungi via telegram (Chat Services LSS)
Reparasi basis gigi tiruan sering menggunakan resin akrilik self-cured yang memiliki kekuatan lentur (flexural strength) rendah sehingga rentan mengalami fraktur. Penelitian ini bertujuan untuk mengetahui pengaruh penambahan nanopartikel zirkonia (nano-ZrO₂) dengan konsentrasi 0,5 wt%, 0,75 wt%, dan 1 wt% terhadap flexural strength resin akrilik self-cured pada reparasi basis gigi tiruan. Penelitian ini merupakan penelitian eksperimental laboratoris dengan desain post-test only control group. Sebanyak 24 spesimen resin akrilik polimerisasi panas berukuran 65 × 10 × 2,5 mm direparasi menggunakan resin akrilik self-cured yang dimodifikasi nano-ZrO₂ dengan konsentrasi 0 wt%, 0,5 wt%, 0,75 wt%, dan 1 wt% (n = 6 per kelompok). Uji flexural strength dilakukan menggunakan metode three-point bending test dengan Universal Testing Machine. Analisis morfologi patahan dan area sambungan reparasi dilakukan menggunakan Scanning Electron Microscope (SEM). Hasil penelitian menggunakan uji one-way ANOVA menunjukkan bahwa penambahan nano-ZrO₂ secara signifikan meningkatkan flexural strength resin akrilik self-cured (p = 0,008). Nilai rata-rata tertinggi diperoleh pada kelompok nano-ZrO₂ 1 wt% sebesar 68,42 MPa, diikuti kelompok 0,75 wt% sebesar 62,22 MPa dan 0,5 wt% sebesar 56,52 MPa, sedangkan kelompok kontrol menunjukkan nilai terendah sebesar 49,51 MPa. Perubahan mode fraktur dari brittle menjadi brittle semi-ductile teridentifikasi pada kelompok resin akrilik yang dimodifikasi nano-ZrO₂. Kesimpulan penelitian menunjukkan bahwa penambahan nano-ZrO₂ dengan konsentrasi 0,5%, 0,75%, dan 1% secara signifikan meningkatkan flexural strength resin akrilik self-cured untuk reparasi basis gigi tiruan, dengan konsentrasi 1 wt% memberikan hasil tertinggi dalam penelitian ini.
Denture base repair is commonly performed using self-cured acrylic resin, which has relatively low flexural strength and is therefore susceptible to fracture. This study aimed to evaluate the effect of zirconia nanoparticles (nano-ZrO₂) at concentrations of 0.5 wt%, 0.75 wt%, and 1 wt% on the flexural strength of self-cured acrylic resin used for denture base repair. This study was an experimental laboratory research with a post-test only control group design. A total of 24 heat-cured acrylic resin specimens measuring 65 × 10 × 2.5 mm were repaired using self-cured acrylic resin modified with nano-ZrO₂ at concentrations of 0 wt%, 0.5 wt%, 0.75 wt%, and 1 wt% (n = 6 per group). Flexural strength testing was performed using the three-point bending test with a Universal Testing Machine. Fracture morphology and repair joint areas were analyzed using a Scanning Electron Microscope (SEM). Data were analyzed using one-way ANOVA followed by the post-hoc Tukey HSD test (α = 0.05). The results showed that the addition of nano-ZrO₂ significantly increased the flexural strength of self-cured acrylic resin (p = 0.008). The highest mean flexural strength was observed in the 1 wt% nano-ZrO₂ group (68.42 MPa), followed by the 0.75 wt% group (62.22 MPa) and the 0.5 wt wt% group (56.52 MPa), while the control group exhibited the lowest value (49.51 MPa). A change in fracture mode from brittle to brittle semi-ductile was observed in the nano-ZrO₂–modified groups. The findings indicate that the addition of nano-ZrO₂ at concentrations of 0.5 wt%, 0.75 wt%, and 1 wt% significantly enhances the flexural strength of self-cured acrylic resin for denture base repair, with the 1 wt% concentration producing the highest improvement in this study.
PENGARUH PENAMBAHAN NANOPARTIKEL ZIRKONIA TERHADAP IMPACT STRENGTH BASIS GIGI TIRUAN RESIN AKRILIK PASCA REPARASI (Cut Zhafirah Haura, 2026)
PENGARUH PENAMBAHAN NANOPARTIKEL ZIRKONIA TERHADAP KEKERASAN BASIS GIGI TIRUAN RESIN AKRILIK PASCA REPARASI (KHANSA NABILA ARINA PUTRI, 2026)
PENGARUH PENGERINGAN AMPAS TEBU SEBAGAI FIBER REINFORCED COMPOSITE TERHADAP FLEXURAL STRENGTH RESIN KOMPOSIT (Win Bramahaga, 2014)
STUDI FLEXURAL STRENGTH RESIN KOMPOSIT FIBER NON-SINTETIK AMPAS TEBU DENGAN DIAMETER YANG BERBEDA (Melvita Dewi, 2014)
PERILAKU MASYARAKAT TERHADAP PEMELIHARAAN KEBERSIHAN GIGI TIRUAN LEPASAN (KAJIAN SURVEI PADA MASYARAKAT GAMPONG PEUNITI BANDA ACEH) (Melisa Idawani, 2023)